The process of making sulphur oil :
· (1) Rub together these two-sulphur 1 sr. and realgar sr. Put the juice of mango 1 sr. into the mixture. If there is the sunshine, put juice otherwise not. Thus do it for a month. If the sunshine is strong, do it, if there is cloud, do not do it. The process pierces seven leaves under and 7 leaves over. True. The process of making the essence of mineral calamine :
(2) Rub mineral calamine 1 sr. in (the juice of) Aloe vera for 7 days, rub it with all these-(the juice of) Vitex trifolia (Nagoại;) next rub it with honey 1, clarified butter, borax 1, sal-ammoniac 1, molasses 1 and gunja 1. Next take it out and take out the essence in the yantra. This is the in process of (the making of) the essence of mineral calamine:
(3) Put the urine of goat 5 srs., the milk of Calotropis gigantea-1 sr. and the milk of Euphorbia niviia (Thohar) 1 sr. into the horse-dung for 21 days. Next take the whole thing out and place it on the fire and give fire of castor plant (Ricinus communis) under it. It gets dried up.
(4) Rub mercury tā. 4, lead tā. 1, sulphur(țā) 1, and sal-ammoniac (ta) 1, in the juice of Doispyros-peregrina (Timbaru) for 7 days. Put the whole thing into a bottle and give it fire. Mix 1 rati of the essence into 1 tola of copper; gold ? (5) The process of wax (Menamundrā) :
Grind all these-Vermillion pai. 1, wax pai. 1, grains of iron pai. 3, magnetic stone pai. 3, Kātbo - (lime mixed with khadir) pai. 1, makha
- pişța (powder of makha). pai. 1, lime pai. 1, lac pai. 1, natron pai. 1 and filter them with a piece of cloth, rub them with the juice of Anacardium. Then there becomes an accomplishment.
Again melting and melting wax 1 sr., pour it into Samudravāri, Thus do it 125 times.
(6) Madanamudrā : pour it into the oil of Anacardium. Again, Mudrā (the process): 1. A kind of mineral,